Providing effective sealing technology solutions for global customers
Customized Special-Shaped Rubber Parts
Description

We could provide each kinds materials and applications rubber parts, including rubber sealing strip, rubber stopper, rubber gasket, rubber keypad and rubber bellow etc. Application range: fire proofing, electric conduction, and food grade etc. IBG could offer sealing scheme as customers' request.

Show Room
Production Confirmation

For non-standard part, we could confirm as customers' drawing or sample. Suitable material could be suggested according to customers' working condition.

Why Choose us

IBG Advantage

The reasons that we could have long-term stable cooperation with our customers: suitable material, innovation strength, strictly quality management and more experience. We have more 20000 molds and large raw material recipe database, could solving each sealing problems.

My company and the customers a solid partnership depends on the achievement of the following aspects: the basic experience material applicability, innovation strength, strict quality management and function integration. Our company has more than 20000 sets of molds with huge database of raw material, processing the sealing problem of seals in various media and various conditions with enough experience.

The procurement division, according to the importance and function of sealing parts, sometimes referred to as C class supplies purchase, in fact the sealing member should belong to a class material. Hydraulic and pneumatic valve seal is the core component technology.

Material Advantage

Cooperation with Dupont, JSR, Dow corning and large raw material recipe database, make our material properties are relatively stable, ensure quality. Rubber formula design ability which make us  meet customers demand better.

Product Inspection & Quality Control

Material Inspection:
Take testing for all storage material, and issue the corresponding raw material property report, meanwhile compare with raw material own property report, two reports property value is consistent, then put into storage.

Mold Inspection:
Die Mold development finished or after cleaning, we will check the full size of the mold, ensure quality for each cavity's product.

Product Inspection:
During production, inspectors will check semi-finished products, ensure product process and make the defective rate control in a reasonable range.

Quality Control:
Quality Department will check product appearance for each batch.

Full Inspection:
Optional Sorting Machine ensure products appearance, 100% qualified.

Technology Requirement
Hardness

Hardness is a physical measure, which is compression deformation degree. Shores hardness is tested by shores durometer, unit " degree"; Two discription: A&D, under 90 degree showed by shores A, over 90 degree showed by shores D. Normal rubber hardness unit is HS and IRHD, value of shores A is same with IRHD.

Temperature

According to working condition, choose suitable material.

Permanent Compression Deformation

One of index for o ring performace is permanent compression deformation of material. Under pressure, o ring elasticity deformed, pressure bigger, will cause permanent compression deformation. Its formula as follows,

Note: b0-oringinal thickness( section dia.)   b1-thick under pressure  b2-thickness after release

Normally, in order to avoid permanent compression deformation, max pressure under static seals is about 30%, under dynamic seal is about 20%.

Failure forms and Solutions
Extrusion

    Description

  • Sealing parts with rough edge, is usually in the low pressure side.

    Reason

  • Clearance/pressure is too large; hardness/elasticity is too low; groove gap is too small; irregular clearance size; improper size of sealing parts.

    Solutions

  • Reducing clearance size, choosing higher hardness or better elasticity material, reasonable groove design.
Twist

    Description

  • Sealing parts become twisting.

    Reason

  • Improper installation, movement speed is too low, material too hard or elasticity too small, improper groove size, rough groove surface.

    Solutions

  • Correct installation, choosing high elasticity material, suitabel groove designation and surface finish, trying to use support ring.
Permanent Compression Deformation

    Description

  • Contacting surface of Sealing parts display permanent deformation.

    Reason

  • Pressure is too large, higher temperature;un-finished sulfuration treatment;material is overexpansion in the chemical medium.

    Solutions

  • Choosing material which is low deformation rate; suitable groove design; confirming materials and medium are compatibility.
Installation Damages

    Description

  • The whole or part of sealing parts appear wound.

    Reason

  • The edge of groove is sharp, size is not suitable. Hardness or elasticity is lower; Surface is dirty.

    Solutions

  • Clear sharp edge; design more reasonable groove designation; choose suitable size; choose more elasticity and higher hardness sealing parts.
Excessive Compression

    Description

  • Sealing parts contacting surface is plane deformation, maybe have crack.

    Reason

  • Unreasonable designation; material deformation, which is caused by heat and chemical medium; or lager pressure.

    Solutions

  • Groove designation shoule consider material deformation, which is caused by heat and chemical medium; or lager pressure.
Heat Corrosion

    Description

  • High temperature contacting surface shown radial crack; maybe material change softer, or material become shiny due to high temperature .

    Reason

  • Material could not bear high temperature, or temperature beyond estimated , or temperature change frequently.

    Solutions

  • Choose high temperature resistance material, if possible, try to reduce temperature of sealing surface.
Electro-corrosion

    Description

  • Seal fade, also have powder residue on the surface .

    Reason

  • Chemical reactions bring electrolysis, unreasonable groove designation, material and medium is incompatible.

    Solutions

  • Choos suitable material with medium, checking groove designation.
Wear

    Description

  • The whole or parts of is wear, material wear particle could be found.

    Reason

  • Surface cleaness is worse, more higher temperature, seal surface treatment is not thorough.

    Solutions

  • Using groove cleaness which is suggested, clean wear pats.
Pressure Blasting

    Description

  • The seal surface appear bubbles, pits, scars; pressure material absorption gas in medium, when the pressure is sulienly reduced, the gas absorbed by the material fast escape. Cause sealing epidermal blasting.

    Reason

  • Pressure changed frequently, hardness and elasticity of material too low.

    Solutions

  • Choose higher hardness and elasticity material, reduce decompression speed.
Chemical Corrosion

    Description

  • Chemical corrosion could cause each kinds defects, such as crack, small hole or color fading, sometimes, chemical corrosion could be tested by instruments.

    Reason

  • Materials and medium does not match, or higher temperature.

    Solutions

  • Choose more chemical resistant material.
Gas evolution

    Description

  • It is difficult to test this flaw, normal form--section size become smaller.

    Reason

  • Improper sulfidizing, hardness too low, or used plasticizer material.

    Solutions

  • Avoid using plasticizer material, assure the sealing parts through correct fluidization process, in order to reduce leakage.
Pollution

    Description

  • Section of sealing parts have dirty matters.

    Reason

  • The producing environment is damaged, material is corrosion, material is non semiconductor industry grade material.

    Solutions

  • Pay attention to cleaness when producing and packing, controlling environment of deliverying and application.